Scratch PyroelectricDetector IndiumTinOxide Chemical_Vapor_Deposition FFM multi_layer ScanningThermalMicroscopy ThinFilm Filter suspended_graphene hard_disk Polyethylene Temasek_Lab FailureAnlaysis INSP Cancer BlockCopolymer Fujian BFO StyreneBeads Piranha norganic Electronics Vac PtfeMembrane Moire NCM Hexylthiophene CuParticle ContactModeDot Polymer medical Blood non_contact MeltingPoint
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Triple-cation perovskite
Scanning Conditions
- System : NX10
- Sample bias: 0 V, 0.5 V
- Scan Mode: C-AFM with PCM toolkit
- Scan Rate : 0.25 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 512×512
- Cantilever : ANSCM-PC (k=0.2N/m, f=12kHz)