AAO MLCC CVD Beads PS_PVAC Ni-FeAlloy Thermoplastic_polyurethane electrospinning cooling LateralForceMicroscopy FrictionalForce align Ucl Tin disulfide Pinpoint Lattice NTU ElectrostaticForceMicroscopy HACrystal Styrene Tape PvdfBead contact ScanningKelvinProbeMicroscopy CaMnO3 dichalcogenide Metal-organicComplex molecular_beam Conduct Phthalocyanine Magnetic Force Microscopy Workfunction multi_layer Yeditepe Array
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fractals of silver nanoparticles
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.31 Hz, 0.27 Hz
- Scan Size : 50μm2, 40μm2
- Pixel Size : All 256×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)