Tungsten_disulfide Yeditepe_University Oxide Floppy Cobalt-dopedIronOxide phase_change 2-vinylpyridine BoronNitride Aluminium_Oxide Nanostructure Cancer FrictionalForceMicroscopy small_scan Composite HexagonalBN MonoLayer InsulatorFilm non_contact PhaseChange Display Au111 INSP HexacontaneFilm CalciumHydroxyapatite OpticalWaveguide strontiu_titanate Trench CntFilm ScanningKelvinProbeMicroscopy Thermal flakes DeflectionOptics Fujian Hole pulsed_laser_deposition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V