PinpointNanomechanicalMode PolyimideFilm Ni-FeAlloy SingleCrystal PvdfBead mechanical property Molybdenum_disulfide ScratchMode DentalProsthesis ScanningThermalMicroscopy HydroGel UnivOfMaryland ScanningTunnelingMicroscopy Conduct doped Pores PVAC Polyvinylidene 2-vinylpyridine Sulfur SKPM Pore VerticalPFM norganic Hexylthiophene Ananth Temperature DIWafer Singapore HighResolution Lattice NtuEee OxideLayer Domain SoftSample
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
STO(SrTiO3), Annealed LAO(LaAlO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm, 5μm×5μm
- Scan Rate: 0.8Hz, .9Hz
- Pixel: 512×512, 256×256