PyroelectricDetector RedBloodCell Treatment Temperature Strontium ConductiveAFM Nanostructure Graphite Ni-FeAlloy PvdfFilm Regensburg Cobalt Sio2 Ram DLaTGS LiBattery polyvinyl acetate ItoGlass FrequencyModulation ferromagnetic molecular_beam multi_layer Thermal SPMLabs Ceramic Potential GaN 2-vinylpyridine MagneticArray Permalloy CeramicCapacitor Terrace MagneticPhase Hexatriacontane Calcium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polyaniline (PANI)
Scanning Conditions
- System: XE7
- Scan Mode: Non-contact
- Cantilever: ACTA (k=40N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512