Metal LateralForceMicroscopy Array Piranha NanoLithography DeoxyribonucleicAcid MagneticPhase Electronics PtfeFilter Platinum Tungsten AlkaneFilm FFM Carbon ULCA SAM #Materials PANI CrossSection nanobar Calcium ContactMode Magnetostrictive HumanHair TPU LightEmission Lattice TungstenThinFilmDeposition AdhesionForce LateralForce Cobalt-dopedIronOxide doped Pinpoint BiVO4 Solar
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ExFoliated graphene on SiO₂/Si wafer
Scanning Conditions
- System : FX40
- Scan Mode: Non-Contact, Lithography
- Scan Rate : 1 Hz
- Scan Size : 10μm×10μm
- Pixel Size : 256×256
- Cantilever : PPP-EFM (k=2.8N/m, f=75kHz)
- Litho. Condition : Force 200nN, Writing speed 0.2 μm/s , AC bias 10 V @ 40 kHz, Humidity ~90% RH