FFM FuelCell Memory phase_change Array Epoxy Styrene Iron MfmPhase BiFeO3 Molybdenum single_layer Heating Etch LiBattery DataStorage AdhesionEnergy DeoxyribonucleicAcid Gallium Logo fluoroaalkane SrTiO3 Pyroelectric Copolymer Lanthanum_aluminate semifluorinated_alkane PinpointPFM Galfenol NCM\ LogAmplifier ThermalProperties BiasMode OpticalWaveguides ImideMonomer Ceramic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
2L-MoS₂ (1/3)
Scanning Conditions
- System : FX40
- Sample bias: 0.25 V
- Scan Mode: C-AFM, LFM
- Scan Rate : 4 Hz
- Scan Size : 2.5μm×2.5μm
- Pixel Size : 512×512
- Cantilever : ContSCPt (k=0.2N/m, f=25kHz)