Kevlar Nanopattern I-VSpectroscopy Optic MeltingPoint Cross-section phase_change Boundary Lift YszSubstrate Au111 Vinylpyridine MagneticPhase HOPG Polyvinylidene PinpointNanomechanicalMode ScratchMode dielectric_trench GaAs Reduction ElectroChemical DIWafer Crystal LightEmiting Nanostructure Gallium_Arsenide ScanningSpreadingResistanceMicroscopy atomic_layer Led ring shape norganic cannabidiol FrictionForce Mfm AtomicLayer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
STO(SrTiO3), Annealed LAO(LaAlO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm, 5μm×5μm
- Scan Rate: 0.8Hz, .9Hz
- Pixel: 512×512, 256×256