Bismuth ElectrostaticForceMicroscopy PVAP3HT OrganicCompound Lateral EPFL StyreneBeads LiquidCrystal cannabidiol mono_layer HBN Korea Wang WPlug Adhesive Iron AtomicLayer Austenite IMT_Bucharest doped BiFeO3 Optoelectronic NUSNNI Stiffness LiBattery pulsed_laser_deposition VerticalPFM Worcester_Polytechnic_Institute frequency_modulation SingleLayer polyvinyl acetate StainlessSteel CntFilm ForceVolumeMapping STO
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferroelectric 2L-hBN
Scanning Conditions
- System : FX40
- Sample bias: 0.25 V, 0.8 V
- Scan Mode: C-AFM
- Scan Rate : 8 Hz
- Scan Size : 1.5μm×1.5μm
- Pixel Size : 256×256
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)