DNA AAO Hair Bmp SThM FloppyDisk semifluorinated_alkanes Molybdenum_disulfide block_copolymer Foil CntFilm Co/Cr/Pt SSRM SolarCell SetpointMode Modulus BlockCopolymer LiBattery Photovoltaics nanomechanical Korea plastics NUS_Physics KPFM Bacteria MagneticPhase LFM Leakage Phase HexagonalBN CancerCell Zagreb exfoliate MetalCompound BiFeO3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li stripping-plating on Li surface
Scanning Conditions
- System : NX10 in dry room
- Scan Mode: Contact/EC AFM
- Scan Rate : 0.15 Hz
- Scan Size : 30μm×30μm
- Pixel Size : 256×256
- Cantilever : Multi75-G
- ECr : Li metal (Working electrode), Li metal (Reference electrode), Li (Counter electrode), 1M LiTFSI in TEGDME (Electrolyte)
- Open circuit voltage : 1 VLi/Li+