Singapore MolecularSelfAssembly medical AdhesionEnergy Solution Reading Inorganic_Compound HumanHair Platinum Water Piezo Trench Pores ScanningIon-ConductanceMicroscopy HanyangUniv PetruPoni Sperm CrAu University_of_Regensburg Electrical&Electronics ScanningKelvinProbeMicroscopy Steps LateralPFM Chemical Vapor Deposition BiFeO3 ScanningTunnelingMicroscopy Hafnia ContactModeDots FAPbI3 LithiumNiobate organic_polymer light_emission Modulus MeltingPoint Adhesion
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
P(VDF-TrFE-CFE)
Scanning Conditions
- System : FX40
- Scan Mode: Tapping
- Scan Rate : 0.5 Hz
- Scan Size : 2μm×2μm
- Pixel Size : 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)