cross section SetpointMode Solar CrossSection DomainSwitching Sapphire Ito StrontiuTitanate semifluorinated_alkane Ni81Fe19 Tape HydroGel ScanningSpreadingResistanceMicroscopy Fluoride Thermoplastic_polyurethane ScanningThermalMicroscopy MembraneFilter Vortex LightEmission Platinum Hafnia Chloroform PolymerBlend C_AFM SingleLayer PANI Treatment PVA VerticalPFM FM-KPFM KAIST HiVacuum Conductance conductive Crystal
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256