Magnets MfmPhase Yttria_stabilized_Zirconia Hexatriacontane DOE Styrene FM_KPFM Treatment CalciumHydroxide ito_film fe_nd_b high_resolution PatternedSapphireSubstrat Magnetic Force Microscopy mfm_amplitude sputter self_assembly Writing PECurve CalciumHydroxyapatite Sadowski AnodizedAluminumOxide Blend OrganicCompound BlockCopolymer Tapping ScratchMode Polarization Polyethylene Granada Array LightEmiting LDPE Workfunction MolybdenumDisulfide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer phase change by temp
Scanning Conditions
- System: NX10
- Scan Mode: Tapping,TCS2
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×256
- Scan Mode: Tapping,TCS2
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×256