nanomechanical Calcite Genetic atomic_steps Annealed AmplitudeModulation Current Ecoli semifluorinated alkane frequency_modulation Wafer medical PVAP3HT HDD MolybdenumDisulfide MagneticArray Polystyrene Leakage LiquidCell Praseodymium Materials GranadaUniv GlassTemperature HOPG ThermalConductivity Mechanical PinPointMode Co/Cr/Pt Writing Heating Topography FloppyDisk AAO Trench OxideLayer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer ΙΙ
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256