ThinFilm Logo Pyroelectric LiquidImaging Polypropylene high_resolution Piranha BCZT cannabidiol ItoGlass Current LightEmission Reduction OpticalModulator DomainSwitching Battery Mechanical ElectroChemical 2d_materials LiIonBattery FailureAnlaysis bias_mode BoronNitride Iron Perovskite Tungsten_disulfide Neodymium ForceMapping #Materials Thermoplastic_polyurethane TungstenThinFilmDeposition Cross-section ForceVolumeMapping Lateral Vinylpyridine
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V