PFM Bismuth Chungnam_National_University cooling GlassTemperature CaMnO3 Ram LMF FailureAnalysis India Growing CNT BlockCopolymer 2-vinylpyridine Styrene #EC SingleLayer CuSubstrate Epoxy Sulfur TCS medical mechanical_property LowDensityPolyethylene SmallScan oxide_layer Formamidinium_lead_iodide Titanate ConductingPolymer Crystal MembraneFilter Hair fe_nd_b ForceMapping domain_switching
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Floppy
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-NCHR (k=80N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel: 256×256
- Scan Mode: CP-AFM
- Cantilever: CDT-NCHR (k=80N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel: 256×256