GaP Austenite HexagonalBoronNitride Cross-section Au111 Ferroelectric phase_change MoS2 Morphology DomainSwitching PhaseImaging VinylAlcohol Wonseok Resistance Calcium PS_LDPE Subhajjit Vac HardDisk frequency_modulation IcelandSpar Calcite semifluorinated alkane Lift Titanate SurfaceOxidation sputter Composite ScanningTunnelingMicroscopy MagneticForceMicroscopy Nanotechnology AIN Chungnam_National_University ContactModeDot TiO2
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 (1/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.1Hz
- Pixel: 512×1024