ring shape LogAmplifier Liquid Vinylpyridine NUS_NNI_Nanocore Mosfet Hafnium_dioxide Ecoli Cross-section Formamidinium_lead_iodide UnivCollegeLondon Permalloy DNAProtein Materials Heat plastic SAM SelfAssembly molecule Bio LeakageCurrent Reading Strontium ForceDistanceSpectroscopy Nanotechnology Polymer mfm_amplitude DNA oxide_layer SicMosfet PVAP3HT Typhimurium vertical_PFM CastIron Magnetostrictive
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Anodized Aluminum Oxide (AAO)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS
- Scan Size: 0.5Hz, 1Hz
- Scan Rate:20μm×20μm, 5μm×5μm
- Pixel: 256 × 256
- Scan Mode: Non-contact
- Cantilever: AC160TS
- Scan Size: 0.5Hz, 1Hz
- Scan Rate:20μm×20μm, 5μm×5μm
- Pixel: 256 × 256