molecules Optic NusEce Tungsten thermoplastic_elastomers KPFM Spincast Sadowski Polyurethane ImideMonomer MagneticForce Piranha Tapping small_scan BaTiO3 Ecoli MechanicalProperties Alloy Dr.JurekSadowski Organic doped Alkane pulsed_laser_deposition Thermoplastic_polyurethane kelvin probe force microscopy HardDiskMedia Crystal TipBiasMode FM_KPFM align TempControl Insulator self-assembly silicon_oxide Mechanical
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512