PANI Oxidation Temperature light_emitting Ceramic Solar Display PolyimideFilm Cobalt CalciumHydroxyapatite Polyurethane BiVO4 Ni-FeAlloy Kevlar TCS Polyvinylidene_fluoride layers Blend Indium_tin_oxide Thermoplastic_polyurethane mfm_amplitude Pattern optoelectronics Blood Dimethicone EFMAmplitude Force-distance MagneticPhase UTEM Composition Austenite frequency_modulation PpLdpe #Materials Pzt
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic device
Scanning Conditions
- System : NX20
- Lift Height : 50nm
- Scan Mode: MFM
- Scan Rate : 0.3Hz
- Scan Size : 20μm×20μm
- Pixel Size : 512×256
- Cantilever : PPP-MFMR (k=2.8N/m, f=75kHz)