StrontiumTitanate InsulatorFilm molecular_beam Cobalt-dopedIronOxide ContactMode BCZT DomainSwitching nanobar cooling Conductive AFM Glass Metal-organicComplex fluoroaalkane conductive Leakage Blend PhaseChange Fujian Ecoli Logo YttriaStabilizedZirconia domain_switching PS_PVAC Scanning_Thermal_Microscopy BariumTitanate ContactModeDot Morphology Calcite UnivCollegeLondon SSRM ElectroChemical AM_KPFM HighAcpectRatio Chloroform Fluoride
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferromagnetic Nanobars Array
Ferromagnetic nanobars arranged on a Penrose P2 tiling. The Permalloy (Ni81Fe19) nanobars are 810 nm and 500 nm long. The width and thickness of a nanobar amount to about 120 nm and 25 nm, respectively.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm