Lateral C36H74 Magnetic electrospinning pulsed_laser_deposition ContactModeDot SiWafer hydrocarbon OpticalWaveguide Cobalt AEAPDES DomainSwitching Force-distance Styrene silicon_carbide Chungnam_National_University DNAProtein TemperatureControlledAFM TempControl AIN Hydroxyapatite Hafnium_dioxide WS2 Melt OrganicSemiconductor Display ScanningIon-ConductanceMicroscopy suspended_graphene Temasek_Lab fluoroaalkane ElectroDeposition biocompatible MoirePattern 2d_materials STM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Perovskite
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36A Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 4μm×4μm
- Scan Rate: 0.3Hz
- Pixel: 512×256