Gold silicon_carbide Logo SPMLabs NtuEee CuSubstrate PANI Reduction SiWafer LiquidCell HighResolution SingleLayer SingleCrystal Trench Battery Steps cross section Pore thermoplastic_elastomers BiVO4 atomic_layer Polydimethylsiloxane Molybdenum_disulfide gallium_nitride STO LiftHeight AM_SKPM nanomechanical SRAM SFAs Praseodymium PinPointMode layers nanobar AM_KPFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic patterned array
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128