lithography Lateral_Force_Microscopy suspended_graphene DOE RedBloodCell NTU margarine medical Plug BismuthVanadate Styrene doped Multiferroic_materials CarbonNanotube MagneticPhase ForceMapping BreastCancerCell Sic InLiquid Praseodymium molecular_beam FM_KPFM PUR Reading Perovskite DomainSwitching Electrode PS_LDPE Metal conductive Writing Conducting MESA structure plastic InorganicCompound
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
SRAM
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 3μm×3μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Sample Bias: 0.5V
- Scan Mode: CP-AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 3μm×3μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Sample Bias: 0.5V